| 139 | 8 | 15 |
| 下载次数 | 被引频次 | 阅读次数 |
介绍了1 100 mm四辊单机架平整机湿平整工艺调整过程及改造内容。通过优选平整液,优化平整压力、平整速度,控制平整液残留、钢卷延伸率和工作辊粗糙度,实现了由干平整模式变为干/湿平整双模式。湿平整模式可实现批量生产MR-2/3/4、SPCC-T4BA、DC03/4/5等多钢种和高硬度、低粗糙度镀锡基板和普冷产品的需求。但因平整液残留导致带钢表面产生斑迹缺陷,仍是湿平整工艺今后攻关方向。
Abstract:This paper introduces the adjustment process and transformation content of the wet leveling process of 1 100 mm four roll single frame leveler.By optimizing the leveling fluid,leveling pressure and speed,controlling the leveling fluid residue,coil elongation and work roll roughness,the dry leveling mode to dry/wet dual leveling mode is realized.The wet leveling mode can meet the requirements of mass production of MR-2/3/4,SPCC-T4 BA,DC03/4/5 and other steel grades,tinned substrates with high hardness and lowroughness and common cold products.However,the spot defect on the strip surface caused by the residue of leveling fluid is still the key research direction of wet leveling process in the future.
[1]张明生.热轧平整机组的板形控制研究[J].河北冶金,2016(10):61~64.
[2]刘志利,张云涛,李晓明,等.河钢邯钢2 180平整机镀铬辊表面色差原因分析[J].河北冶金,2020(6):72~74.
[3]白振华,韩林芳,高健,等.干平整中工作辊与带钢表面粗糙度对摩擦系数影响的研究[J].燕山大学学报,2012,36(01):18~21+26.
[4]白振华,朱厚鸿,代东东,等.VC辊平整机组湿平整过程关键轧制工艺参数的优化设定[J].塑性工程学报,2014,21(04):92~96.
[5]魏圣明,周为民.某连退机组湿平整改造[J].机械工程与自动化,2013(3):211~212+214.
[6]Brauneis Robert,Steinboeck Andreas,Jochum Martin,Kugi Andreas. Model-based dynamic calibration of a multi-actuator gap leveler for heavy plates[J]. Journal of Manufacturing Science and Engineering,2020,142(7):25~27.
[7]白振华,李麒麟,钱承,等.湿平整过程中平整液流量差异性优化设定技术[J].塑性工程学报,2016,23(05):77~82.
[8]钱承,张佳胜,白振华,等.二次冷轧轧辊表面油膜厚度模型及其影响因素[J].钢铁,2020,55(06):68~74.
基本信息:
DOI:10.13630/j.cnki.13-1172.2022.0114
中图分类号:TG335
引用信息:
[1]王文宝,冯哲,刘建龙,等.1100 mm四辊单机架湿平整工艺改造[J].河北冶金,2022,No.313(01):69-72.DOI:10.13630/j.cnki.13-1172.2022.0114.
2022-01-28
2022-01-28